Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 12.92 g/cc | 0.4668 lb/in³ | |
CMW® ELKONITE® G14 Tungsten Carbide Silver contact material ASTM 663, Class A, infiltrated For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |