Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 11.78 g/cc | 0.4256 lb/in³ | |
Wall Colmonoy COLMONOY® 83 PTA - Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide Description and Application: A tough nickel-chromium-tungsten-boron matrix alloy containing chromium carbides with the addition of extremely hard tungsten-carbide particles for excellent abrasive we.. |