Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 10.36 g/cc | 0.3743 lb/in³ | |
Indium Corp. Indalloy 63 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 10.36 g/cc | 0.3743 lb/in³ | |
Indium Corp. Indalloy® 233 Pb-Sb-Sn Solder Alloy Intermediate temp solder. Creep resistant.Information provided by the manufacturer, Indium Corporation. |