Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 10.2 g/cc
0.368 lb/in³
Hogen Duralloy H100M Molybdenum
RWMA Class 13.Typical Resistance Welding Applications: H100M is not as hard as H100W (pure tungsten) and can be drilled or machined to fit parts to be joined. It may be used much the same as H100W ..
Density >= 10.2 g/cc
>= 0.368 lb/in³
H.C. Starck Glass Melting Electrodes made from Electron Beam Melted Molybdenum
Description of Product: The electrodes are manufactured by electron beam melting from pure molybdenum and are supplied to customer requirements by forging or machining.Range of Application: Electr..
Density >= 10.2 g/cc
>= 0.368 lb/in³
H.C. Starck Pure Molybdenum Tube Powder Metallurgy Targets
This specification covers extruded molybdenum tubes produced from pressed and sintered powder metallurgy billet for sputtering applications.Information provided by H.C. Starck.
Density 10.2 g/cc
0.368 lb/in³
ASTM D792
Techmer ES HiFill® PA6 1020
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Density 10.2 g/cc
0.368 lb/in³
Wieland 3011 Wilaform Silver
Universally applicable silver alloyApplications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Density 10.2 g/cc
0.368 lb/in³
CMW® ELKONIUM 217 Silver Cadmium Alloy
The alloying of silver with cadmium produces materials with good arc extinction, good corrosion resistance and low contact resistance characteristics and provides them with good switching capability..
Density 10.2 g/cc
0.368 lb/in³
Cadi 100M Molybdenum
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.
Density 10.2 g/cc
0.368 lb/in³
Cadi Molybdenum
Molybdenum is suited for high temperature applications with good corrosion resistance, workability, and a low coefficient of thermal expansion.Information provided by Cadi Company.