Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.01 g/cc | 0.326 lb/in³ | |
Indium Corp. Indalloy 17 Low Melting Bismuth Alloy Information Provided by Indium Corporation |
|||
Density | 9.03 g/cc | 0.326 lb/in³ | |
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative.. |
|||
Density | 9.01 g/cc | 0.326 lb/in³ | |
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 9.01 g/cc | 0.326 lb/in³ | |
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Density | 9.01 g/cc | 0.326 lb/in³ | |
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Density | 9.03 g/cc | 0.326 lb/in³ | |
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is .. |