Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.68 g/cc | 0.314 lb/in³ | |
Indium Corp. Indalloy 113 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, GTAW, as welded, notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Density | 8.68 g/cc | 0.314 lb/in³ | |
Williams Advanced Alloys WS200 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | Annealed |
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | Annealed |
Eagle Brass 770 Nickel Silver 18%, 1/4 Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | Annealed |
Eagle Brass 770 Nickel Silver 18%, Annealed 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | Annealed |
Eagle Brass 770 Nickel Silver 18%, Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, GMAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, GTAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Density | 8.69 g/cc | 0.314 lb/in³ | |
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |