Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.49 g/cc | 0.307 lb/in³ | deposit density |
Kennametal Stellite Deloro® 22 Nickel Alloy Deloro™ 22 is a pre-alloyed gas atomized nickel based powder which is used primarily for the local repair and hardfacing of glass forming molds. It can also be used as a tough build-up alloy fo.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | P/M (98%) |
Kennametal Stellite Stellite® 190 PM with P/M Processing Adhesive wear test data: P/M 0.32.Applications: vane plugs, fuel metering pins, spacer bushings, ball (bearings) blanks, race (bearings) blanks, diesel engine exhaust, fluid valve seats, saw cutter .. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Lucas-Milhaupt 63 Sn-37 Pb Tin/ Silver Solder Characteristics:Although widely used in electronics for both manual and automatic soldering applications, it is also used in general purpose applications where fast alloy flow is desired. This allo.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Indium Corp. Indalloy 109 Tin-Lead Solder Alloy Good electrical grade solderInformation Provided by Indium Corporation |
|||
Density | 8.49 g/cc | 0.307 lb/in³ | |
Indium Corp. Indalloy 25 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | at RT |
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Wieland 1104 Wilaform Gold Silver white gold alloy for all kinds of decoration manufacturing.Applications: casting, chains, coin/shape, laminar decorationDental |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Williams Advanced Alloys WS188 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 8.50 - 8.70 g/cc | 0.307 - 0.314 lb/in³ | |
Goodfellow T2-Thermocouple Alloy The negative element of the type K thermocouple, the positive being T1. The thermocouple can be used up to 1250C in oxidizing atmospheres, and probably is the most common in use.Information provided.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Goodfellow T1-Thermocouple Alloy The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also .. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Chicago Extruded Metals UNS C36000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Chicago Extruded Metals UNS C36010 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Wall Colmonoy COLMONOY® 42 SA - Hard Nickel-Chromium-Boron Alloy Containing Chromium Carbides Description and Application: Similar to Colmonoy No. 52 SA, but better ductility, less hardness, and slightly less abrasion and corrosion resistance. Finished by carbide tools and grinding.Method o.. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | theoretical |
Wall Colmonoy COLMONOY® 57 PTA - Nickel-Base Hard-Surfacing Alloy Description: Colmonoy 57 PTA is a unique Ni-Cr-B alloy containing optimized amounts of precipitated tungsten rich hard phases distributed throughout the matrix. These hard phases offer substantial .. |
|||
Density | 8.50 g/cc | 0.307 lb/in³ | |
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |