Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.10 g/cc | 0.293 lb/in³ | RT |
Outokumpu 4529 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Kennametal Stellite Nucalloy® 453 High-Silicon Nickel-Base Hardfacing Alloy Applications include chemical control valves, nuclear globe valves, nuclear gate valves, nuclear sliding parts, and pressure bars for plywood cutters.Nucalloy® alloys are unique, patented, high-s.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy Applications include diesel engine valves, and injection mold screws.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinati.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43 Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals INCONEL® Alloy 601 A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals NILO® 365 Controlled-Expansion Alloy For the manufacture of tooling for composites, the NILO® nickel-iron alloys offer a unique combination of matched thermal expansion to avoid warping during the curing cycle, along with strength, .. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals NILO® Alloy 36 Low-Expansion Alloy Inflection point 220°C. A nickel-iron low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coeffic.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Goodfellow Evanohm® Precision Resistance Nickel Alloy Electrical resistance alloy with a very low temperature coefficient of resistivityInformation provided by Goodfellow. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications Properties: Tungs ten-molybdenum high speed steel with ex cel lent toughness and cut ting proper ties, for a wide variety of uses.Applications: Taps, twist drills, reamers, broaching tools, meta.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Bales Mold Service Nibore® Electroless Nickel - Boron Nitride Mold Coating Nibore® is an electroless nickel phosphorus coating that incorporates boron nitride particles in a co-deposited nickel matrix. This unique process is formulated to produce a uniformly dispersed bor.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
California Fine Wire Stablohm 800 Nickel, Chromium, Aluminum, and Copper Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
ATI Allvac® Nickelvac® N-90 Nickel Superalloy, Heat Treatment: 1066°C (1950°F) + Age Data provided by Allvac.Applications: Turbine blades and other jet engine components. Valves for internal combustion engines. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Bohler-Uddeholm BÖHLER S500(m42) High Speed Steel Description: Cobalt Molybdenum high speed steel processing high hardness, excellent cutting properties, high red hardness and good toughness. BOHLER S500 is also available in the special grade ISORA.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness .. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Carpenter Glass Sealing "42-6" Alloy A nickel-chromium-iron which has been developed to match the thermal expansion characteristics of 0120 glass. An additional advantage of this alloy for glass-to-metals seals is the tight dark green.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |