Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel SIRIUS 800 H+ Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42 Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0... |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Lucas-Milhaupt SIL-FOS 2 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 2 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Lucas-Milhaupt Silvalite Brazing Alloy SILVALITE is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on v.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Latrobe Marvac 250 VIM-VAR ; 10 in. High Strength Maraging Steel MARVAC 250 VIM-VAR is a low carbon maraging steel capable of 240,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Indium Corp. Indalloy 110 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Lucas-Milhaupt Silvaloy® 2 Brazing Alloy Silvaloy 2 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica.. |
|||
Density | 8.01 g/cc | 0.289 lb/in³ | |
Wall Colmonoy COLMONOY® 56 PTA - Nickel-Base Hard-Surfacing Alloy With Chromium Boride Description: Colmonoy 56 PTA is a premium alloy specially formulated for plasma transferred arc (PTA) application on new and worn extrusion screws. High levels of chromium and carbon produce large .. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel Description: Molybdenum high speed steel with high toughness and good cutting ability. Applications: Taps, twist drills, reamers, milling tools, broaches toolsStandards: DIN/EN 1.3346 HS2-91, AISI M.. |
|||
Density | 7.99 g/cc | 0.289 lb/in³ | |
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LXN™ (UNS S31726) Allegheny Ludlum's 317LXN™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allvac® VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age Data provided by Allvac.Applications: Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allvac® VascoMax® T-200 Specialty Steel Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts.Property values are for samples in the metallurgical condition: 1500°F age.Informat.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allvac® VascoMax® T-250 Specialty Steel, Heat Treatment: 816°C (1500°F) + Age Data provided by Allvac.Applications: Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts. |