Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.92 g/cc | 0.286 lb/in³ | Sintered |
Kinetics MIM 316 Stainless Steel (Premium Grade) Austenitic stainless steel. Excellent corrosion resistance. Excellent elongation. Non-magnetic. Easily weldable. Can be polished to a mirror finish. Provides better elongation and ductility over the.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | |
Latrobe DuraTechâ„¢ M4 High Carbon Powder Metal High Speed Steel (ASTM M4) DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | |
Latrobe DuraTechâ„¢ M4 Powder Metal High Speed Steel (ASTM M4) DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v.. |
|||
Density | 7.93 g/cc | 0.286 lb/in³ | |
Special Metals BRIGHTRAY® Alloy 35 Electrical Resistance Alloy A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 1920°F (1050°C). It is similar to BRIGHTRAY alloy F but with rare-earth additions for greater resist.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | |
Special Metals UDIMET® Alloy 250 Maraging Steel A high-strength, maraging steel of iron and nickel with additions of molybdenum and titanium. It has the strength of standard 18Ni (250) maraging steel but the advantages of containing less molybde.. |
|||
Density | 7.93 g/cc | 0.286 lb/in³ | |
Wall Colmonoy COLMONOY® 6 PTA Nickel-Base Hard Surfacing Alloy With Chromium Boride Description: Optimized formulation to offset dilution and alloy loss from the arc. Designed for PTA Application.Applications: Colmonoy 6 PTA is designed for plasma transferred arc (PTA) application... |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 305 Austenitic Stainless Steel, 1/2 Hardened Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 305 Austenitic Stainless Steel, 1/4 Hardened Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 305 Austenitic Stainless Steel, Annealed Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316 Austenitic Stainless Steel, 1/2 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316 Austenitic Stainless Steel, 1/4 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316 Austenitic Stainless Steel, 1/8 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316 Austenitic Stainless Steel, 3/4 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316 Austenitic Stainless Steel, Annealed The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316 Austenitic Stainless Steel, Full Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316L Austenitic Stainless Steel, 1/2 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316L Austenitic Stainless Steel, 1/4 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316L Austenitic Stainless Steel, 1/8 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316L Austenitic Stainless Steel, 3/4 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316L Austenitic Stainless Steel, Annealed Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | As Annealed |
Eagle Brass 316L Austenitic Stainless Steel, Full Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | |
Crucible Steel REX® M4 High Speed Steel REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punch.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | |
Crucible Steel REX® TMO High Speed Steel, AISI M1 REX TMO molybdenum-tungsten high speed steel is a tough general purpose high speed steel with high cutting efficiency and excellent finishing properties. It is adapted to fast light cuts on soft or .. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | soft annealed |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
Density | 7.91 g/cc | 0.286 lb/in³ | |
ATI Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age Data provided by Allvac.Applications: Discs, rings, bolts for gas turbines. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | |
ATI Allvac® Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: Jet engines, superchargers, missile components, fasteners, cryogenic equipment, nuclear, corrosive deep well hardware. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | Solution Treated |
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286 Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at .. |
|||
Density | 7.93 g/cc | 0.286 lb/in³ | RT |
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |
|||
Density | 7.92 g/cc | 0.286 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 321 (UNS S32100) AL 321 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |