Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Density | 7.80 - 8.00 g/cc | 0.282 - 0.289 lb/in³ | |
Pacific Sintered Materials BZ-111-UC Yellow Brass Powdered Metal Applications: 80-20 leaded brass, coined for close dimensional control, strength and density.Equivalent MPIF Specification: CZP-2000-12All information provided by Pacific Sintered Metals. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel Superplast® 400 High Hardness Mold Steel SUPERPLAST® 400 is an injection plastic mold steel pre-hardened to a high level of hardness. It is delivered at a typical hardness of 125 kg/mm2. This steel is specially adapted for heavy-duty .. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (593°C - 4 hours + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corr.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | ASTM D792 |
Techmer ES HiFill® TPU 0780 Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
CeramTec Sonox® P508 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Goodfellow Cobalt/Boron/Silicon/Iron/Molybdenum/Nickel Alloy Information provided by Goodfellow. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Crucible Steel CPM® 3V® Tool Steel CPM 3V is a new tool steel made by the Crucible Particle Metallurgy process, designed to provide maximum resistance to breakage and chipping in a highly wear-resistant steel. CPM 3V offers impact to.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Crucible Steel CRU-WEAR® Tool Steel CRU-WEAR is an air-hardening tool steel, heat treatable to HRC 60-65. Designed as an upgrade to D2, it offers better wear resistance, greater toughness and higher attainable hardness. Compared to th.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | hardened to 57 HRC |
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type AL 436S™ Ferric Stainless Steel The AL 436S™ alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Angular titanium carbo-nitiride particles occur randomly in the ferrite matrix mi.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1075 (Heated 579°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | ASTM D792 |
3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing Parts fabricated from this rapid prototype metal material are actually a blend of stainless steel and bronze. The part is built with steel and subsequently infiltrated with bronze. A6 is great for .. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |
|||
Density | 7.81 g/cc | 0.282 lb/in³ | |
Latrobe Dynamax™ ASTM M42, DIN 1.3247 Super High Speed Steel Dynamax super high speed steel is a premium cobalt high speed steel with a chemical composition designed for high hardness and superior hot hardness. These properties make the steel an excellent cho.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (593°C - 4 hours - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |