Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide s.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420) TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe LSSâ„¢ 420 Supreme Plastic Mold Steel (AISI 420) TLS 420 Supreme is a specially-refined, mold-quality stainless steel that is engineered to provide supreme polishability, good corrosion resistance, and good wear resistance. TLS 420 supreme is manu.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe BG42® Stainless Knife Steel (AMS 5749) LESCALLOY® BG42® VIM VAR is a double vacuum melted martensitic stainless high speed steel designed for critical aerospace structural components and high performance bearings. The steel is vacu.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe CBS-223â„¢ VIM-VAR Carburizing Bearing and Gear Steel CBS-223 VIM-VAR steel is a double vacuum melted carburizing steel with high hot hardness characteristics. Double vacuum melting sequentially combines vacuum induction melting with VACARCâ„¢ remel.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® 52100 VAC-ARC High Performance Bearing Steel LESCALLOY 52100 VAC-ARC is a deep hardening alloy steel used for aircraft bearings and other high stressed parts where good rolling contact fatigue strength is required at operating temperatures bel.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Viscount 44® Prehardened Tool Steel (ASTM H13S) Viscount 44 is a free-machining, prehardened, H13-type hot work tool steel. It is produced using special melting, forging, and heat treating processes which provide the optimum in control
and reprod.. |
|||
Density | 7.74 g/cc | 0.280 lb/in³ | |
CeramTec Sonox® P502 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | A |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel LABELLE® Silicon #2 Tool Steel LaBelle Silicon #2 is a shock resisting tool steel capable of maximum toughness at relatively high hardness. It has excellent resistance to impact and battering, with good edge retention.Information.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b.. |
|||
Density | 7.74 g/cc | 0.280 lb/in³ | |
AK Steel 420 ULTRA HONE® Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Density | 7.75 g/cc @Temperature 200 °C |
0.280 lb/in³ @Temperature 392 °F |
|
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 43.6% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930 Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive .. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 444™ Ferritic Stainless Steel Low carbon, low nitrogen ferritic stainless steel alloy. Characteristics:practically immune to chloride stress corrosion cracking, enhanced resistance to pitting and crevicing, good general corrosi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® Vasco® M152 Specialty Steel, Heat Treatment: 691°C (1275°F) Anneal Data provided by Allvac.Applications: Rings and structural components for land-based turbines. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® VascoJet® 1000 Specialty Steel, Heat Treatment: 1010°C (1850°F) Q+T Data provided by Allvac.Applications: Landing gear components, springs, fasteners. Gears and shafts for helicopter applications. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1025 Precipitation Hardening Alloy Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum E-BRITE 26-1® Superferritic Stainless Steel, UNS S44627 Property data below is typical of annealed samples. High purity superferritic stainless steel. Available in sheet and strip for use in chemical process equipment to combat chloride pitting and stre.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Schmolz + Bickenbach Cryodur® 2357(S-7) Cold Work Die Steel Description: Cryodur 2357 is a shock resistant tool steel with excellent toughness and high strength; Suitable for cold and hot work applications up to 1000 °F; and Supplied in the annealed conditi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® HY-180 VIM-VAR ; 4.01 - 8.00 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Schmolz + Bickenbach Formadur® 2085 Plastic Mold Steel Description: FORMADUR 2085 is a free-machining corrosion-resistant mold frame steelCharacteristics: Lower mold production costs due to improved machinability; Improved corrosion resistance compared .. |
|||
Density | 7.75 g/cc @Temperature 191 °C |
0.280 lb/in³ @Temperature 375 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |