Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.70 g/cc | 0.278 lb/in³ | RT |
Outokumpu 4501 Duplex Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | RT |
Outokumpu 4713 High Temperature Ferritic Stainless Steel Does not form brittle phases but should only be exposed to moderately corrosive atmospheres due to low chromium content.Applications: Mostly used in high temperature applications with sulphurous atm.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
PSM Industries PolyAlloys MIM-Fe-50%Co Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Piezo Kinetics 406 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars. PKI 406 is suitabl.. |
|||
Density | 7.69 g/cc | 0.278 lb/in³ | Sintered |
Kinetics MIM 440C Stainless Steel Martensitic stainless steel. Excellent strength, hardness, and wear resistance while offering some corrosion resistance. Magnetic. Often used for automotive, cutlery, industrial equipment, power han.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
CeramTec Sonox® P6 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | As Annealed |
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Density | 7.70 g/cc @Temperature 200 °C |
0.278 lb/in³ @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Density | 7.70 g/cc @Temperature 300 °C |
0.278 lb/in³ @Temperature 572 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Density | 7.70 g/cc @Temperature 399 °C |
0.278 lb/in³ @Temperature 750 °F |
hardened to 57 HRC |
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | hardened to 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
AK Steel 409Ni Ferritic Stainless steel AK Steel 409Ni is a nominal 11% chromium stainless steel micro-alloyed with titanium, manganese and nickel that provides excellent weldability, toughness and fabricating characteristics. AK Steel 4.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Stress Relieved Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Carpenter Chrome Core® 8 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | Typical |
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition C AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Carpenter Chrome Core® 8-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 30% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 70% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Latrobe LSS™ PGK Knife and Die Steel TLS PGK knife and die steel is a versatile medium-chromium, air-hardening tool steel that is characterized by a very good combination of toughness and wear resistance. It is available primarily in f.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 2 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.70 g/cc @Temperature 399 °C |
0.278 lb/in³ @Temperature 750 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |