Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.63 g/cc | 0.276 lb/in³ | |
Indium Corp. Indalloy 13 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Schmolz + Bickenbach 416RS Stainless Steel Bar Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | Coating Property |
The NanoSteel® Company SHS 7574 HVOF Steel Alloy, Atomized Powder Coating Description: SHS 7574 HVOF is an iron based steel alloy with a nanoscale microstructure that features extreme corrosion resistance in high chlorine, salt fog, concentrated salt and seawater .. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Crucible Steel CSM® 420 XL Stainless Steel CSM 420 XL is the workhorse premium quality stainless mold steel designed for applications requiring a combination of corrosion resistance and wear resistance. It is double melted for the microstruc.. |
|||
Density | 7.64 g/cc @Temperature 199 °C |
0.276 lb/in³ @Temperature 390 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Relay Steels No. 5 Silicon and iron alloyApplications:relays, armatures, solenoids, magnetic clutches, pole pieces, certain types of motors, transformers, data processing equipment.Information provided by Allegheny Lu.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ArcelorMittal Torque 20-15 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
CeramTec Sonox® P4 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Annealed Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 288°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 316°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 427°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 538°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC Allegheny Ludlum Type 410HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |