Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.57 g/cc | 0.273 lb/in³ | |
MarkeTech NB:WO (Sodium Bismuth Tungstate, NaBi(WO4)2) Scintillator Crystal Double tungstate of sodium and bismuth NaBi(WO4)2 (NBWO) is also a new "heavy", "fast" and optically dense oxide single crystal. Is used as a Cherenkov radiator.Data provided by the supplier, MarkeT.. |
|||
Density | 7.57 g/cc | 0.273 lb/in³ | |
MarkeTech Neodymium Gallium Oxide (NdGaO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 1.2%. |
|||
Density | 7.55 g/cc | 0.273 lb/in³ | |
Indium Corp. Indalloy 118 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.57 g/cc | 0.273 lb/in³ | |
Ferro EG 2791 Thick Film Glass Glass Type: Bi-Pb-Zn Typical Powder Form: MVG Typical Application: End Termination Ferro produces standard and custom glass products that are used in thick film compositions including resistors, co.. |
|||
Density | 7.57 g/cc | 0.273 lb/in³ | |
Mateck Neodymium Gallate Substrate, NdGaO3 Substrate single crystals for superconductivity |
|||
Density | 7.55 g/cc | 0.273 lb/in³ | |
Williams Advanced Alloys WS213 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.56 g/cc | 0.273 lb/in³ | |
Assab Steels VANADIS 4 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:High wear resistanceHigh compressive strengthVery good through-hardening propertiesVery good toughnessExcellent di.. |
|||
Density | >= 7.55 g/cc | >= 0.273 lb/in³ | |
Channel Industries 5800 Lead Zirconate Titanate Piezoelectric Characterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extensively used .. |
|||
Density | >= 7.55 g/cc | >= 0.273 lb/in³ | |
Channel Industries 5400 Lead Zirconate Titanate Piezoelectric Navy Type ICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extens.. |
|||
Density | >= 7.55 g/cc | >= 0.273 lb/in³ | |
Channel Industries 5804 Lead Zirconate Titanate Piezoelectric Navy Type IIICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exte.. |