Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.24 g/cc | 0.262 lb/in³ | |
Indium Corp. Indalloy 172 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.26 g/cc | 0.262 lb/in³ | |
Indium Corp. Indalloy 173 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.26 g/cc | 0.262 lb/in³ | |
Indium Corp. Indalloy® 131 97Sn/3Sb Lead-Free Solder Alloy Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.25 g/cc | 0.262 lb/in³ | |
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â.. |
|||
Density | 7.24 g/cc | 0.262 lb/in³ | |
Indium Corp. Indalloy 259 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.25 g/cc | 0.262 lb/in³ | |
Indium Corp. Indalloy® 227 Sn-In-Ag Solder Alloy Pb free solder can be used as a replacement for 63Sn 37Pb, 62Sn 36Pb 2Ag and 60Sn 40Pb in that it has similar physical and mechanical properties. Not for use over 100°C due to 118°C Sn/In eut.. |
|||
Density | 7.25 g/cc | 0.262 lb/in³ | |
Special Metals INCOLOY® Alloy MA 956 An iron-chromium-aluminum alloy that is oxide dispersion strengthened and produced by mechanical alloying. Production involves high-energy milling of metal powders to create an alloy with a strengt.. |
|||
Density | 7.25 g/cc | 0.262 lb/in³ | |
Williams Advanced Alloys WS187 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.25 g/cc | 0.262 lb/in³ | |
Williams Advanced Alloys WS240 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.24 g/cc | 0.262 lb/in³ | |
American Elements Neodymium Oxide Nanopowder General DescriptionND-MITE powders and dispersions are inorganic neodymium-oxide nanoparticles. ND-MITE-A products are uncoated and hydrophilic. ND-MITE-O products are coated with an organic silane .. |
|||
Density | 7.25 g/cc | 0.262 lb/in³ | |
Crucible Steel CPM® 15V® Tool Steel CPM 15V is intended for applications requiring exceptional wear resistance. It has more vanadium carbides in its microstructure than CPM 10V and provides more wear resistance and longer tool life in.. |
|||
Density | 7.25 g/cc | 0.262 lb/in³ | |
California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 7.25 g/cc | 0.262 lb/in³ | |
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |