Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.20 - 7.60 g/cc | 0.260 - 0.275 lb/in³ | |
Pacific Sintered Materials F-241-T Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-20All information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
Pacific Sintered Materials F-241-T Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE V, CLASS AAll information provided by Pac.. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
Pacific Sintered Materials FN-253-T(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-140HTAll information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
Pacific Sintered Materials FN-262-T High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-45All information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
Pacific Sintered Materials FN-262-T(HT) High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0408-155HTAll information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
Pacific Sintered Materials FX-226-T Infiltrated Iron Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1000-25All information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
Pacific Sintered Materials FX-227-T Infiltrated Steel Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1005-50All information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
Pacific Sintered Materials FX-232-T(HT) Infiltrated High Carbon Steel Powdered Metal Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-110HTAll information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
Pacific Sintered Materials FX-233-T Infiltrated Alloy Steel Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
Pacific Sintered Materials FX-233-T(HT) Infiltrated Alloy Steel Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
PSM Industries Pacific Sintered Metals 4600 F-253-T(HT) Powdered Metal High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-140HTInformation Provided by Pacific Sintered Metals, a division of PSM .. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-256-T(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0408-155HTInformation Provided by Pacific Sintered Metals, a divis.. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
PSM Industries Pacific Sintered Metals Infiltrated Alloy Steel FX-233-T Powdered Metal Excellent combination of strength and shock resistance, Good for use in cams, pawls, sprockets and wear plates, Moderate tolerance controlInformation Provided by Pacific Sintered Metals, a division .. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T(HT) Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-110HTInformation Provided by Pacific Sintered Metals, a division of PSM Industri.. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
PSM Industries Pacific Sintered Metals Infiltrated Iron FX-226-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1000-25Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
PSM Industries Pacific Sintered Metals Infiltrated Steel FX-227-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1005-50Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Density | 7.20 - 7.60 g/cc | 0.260 - 0.275 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.20 g/cc | 0.260 lb/in³ | |
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S.. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division.. |
|||
Density | 7.20 g/cc | 0.260 lb/in³ | |
IBC Advanced Alloys 6% BeNi Beryllium Nickel Master Alloy Beryllium nickel “Master Alloys†are formulated to introduce relatively small percentage “alloying†additions to base metal furnace melts. Producers of aluminum, magnesium, and n.. |
|||
Density | 7.20 g/cc | 0.260 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C62500 Aluminum Bronze Finished product available in rods.Chicago Extruded Metal temper code: M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals |
|||
Density | 7.20 g/cc | 0.260 lb/in³ | |
China Tungsten NT6 Titanium Carbide and Nitride Based Carbides Semi-finishing of low carbon steel, low alloy steel, gray cast iron, Si-AL alloy and finishing of stainless steel.Information provided by China Tungsten |
|||
Density | 7.20 g/cc | 0.260 lb/in³ | |
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Density | 7.20 g/cc | 0.260 lb/in³ | |
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48 Dura-Bar G1 contains flake graphite in a matrix that is pearlitic with small amounts of ferrite. This is the softest grade of the Dura-Bar gray irons and is normally selected when excellent machinab.. |
|||
Density | 7.20 - 7.80 g/cc | 0.260 - 0.282 lb/in³ | |
China Tungsten ST2175 PM Antifriction Parts Information provided by China Tungsten |
|||
Density | 7.20 g/cc | 0.260 lb/in³ | |
Anderman Ceramics EREC99 Cerium Oxide Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met.. |
|||
Density | 7.20 - 7.50 g/cc | 0.260 - 0.271 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type V, Class AInformation Provided by Pacific Sintered Metals, a di.. |