Polymer Property : Density = 0.187 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 5.18 g/cc
0.187 lb/in³
Schott SF6 Glass
Information Provided by SCHOTT North America, Inc.
Density 5.18 g/cc
0.187 lb/in³
Schott SF6HT Glass
Information Provided by SCHOTT North America, Inc.