Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.89 g/cc | 0.177 lb/in³ | |
MarkeTech Barium Fluoride, BaF2 Scintillator Crystal Data provided by the supplier, MarkeTech International. |
|||
Density | 4.90 g/cc | 0.177 lb/in³ | ASTM-C 20 |
CoorsTek DuraSense™ Ceramic Alumina Toughened Zirconia Oxygen ionic conductor for extreme-stress and extreme-thermal-shock environments |
|||
Density | 4.90 g/cc | 0.177 lb/in³ | |
BASF Sicopal® Green K 9610 Color Additive Chemical Structure: Co/Ti/Ni/Zn-oxideApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA PETP, CA/CAB and UPRecommendations for food applicat.. |