Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.24 g/cc | 0.153 lb/in³ | |
Schott P-SF67 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Density | 4.24 g/cc | 0.153 lb/in³ | |
Schott N-LAF34 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.23 g/cc | 0.153 lb/in³ | |
American Elements T-MITE™ Titanium Oxide Nanopowder General DescriptionT-MITE™ powders and dispersions are recently developed inorganic titanium dioxide nanoparticles which impart special UV filtering and reflective properties to coatings and surfac.. |