Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.86 - 3.94 g/cc | 0.139 - 0.142 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9915 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Density | 3.86 - 3.92 g/cc | 0.139 - 0.142 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9922 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.85 g/cc | 0.139 lb/in³ | |
GBC Grade 99 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Density | 3.85 g/cc | 0.139 lb/in³ | |
ICE Al2O3 99.5 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Density | 3.84 g/cc | 0.139 lb/in³ | |
Schott KZFS12 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.86 g/cc | 0.139 lb/in³ | |
Schott N-PK51 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Density | 3.84 g/cc | 0.139 lb/in³ | |
Schott N-LAK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.86 g/cc | 0.139 lb/in³ | |
Schott SF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.85 g/cc | 0.139 lb/in³ | |
CoorsTek StatSafe™ ADC Static Dissipative Alumina Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes.. |
|||
Density | 3.84 g/cc | 0.139 lb/in³ | |
Anderman Ceramics EA995 Sintered Alumina, 99.5% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Density | 3.86 g/cc @Temperature 20.0 °C |
0.139 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals (CsAlF-Complex) Cesium Fluoroaluminate Low-melting-point flux for brazing aluminum.HS No.: 38109090 /CAS-No.: 138577-01-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appl.. |