Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.10 g/cc | 0.112 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight .. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
NanoScale NanoActive® Calcium Oxide Plus NanoActive CaO Plus is produced using proprietary processes to obtain high specific surface area (over 90 m²/g vs. 1-2 m²/g for standard CaO), small crystallite size material possessing high chemi.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Parker Chomerics CHO-LUBE 4220 Electrically Conductive Grease CHO-LUBE 4220 conductive grease is based on silicone fluid, which is characterized by unusual chemical inertness and outstanding thermal stability. It is a silver-filled lubricant designed for surfa.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
MMCC Al/Al2O3 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Mo-Sci Corporation GAI-40-I Green A Intruder Filter Glass Applications: Lead-free NVIS Green A Intruder filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Schott G018-090 Dental Glass Remarks: High fluoride and Zn-containing Sr-glassApplication: Glass ionomer cement, CompomerAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacities.. |
|||
Density | 3.11 g/cc | 0.112 lb/in³ | |
Schott N-BALF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Sapco Si.SiC Silicon Carbide Information provided by Sapco. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Schott G018-117 Dental Glass Remarks: High fluoride and Zn-containing Sr-glassApplication: Glass ionomer cement, CompomerAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacities.. |
|||
Density | 3.11 g/cc | 0.112 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
UBE Tyranno Grade SA Ceramic High Temperature Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | DIN EN 623-2 |
CeramTec CD 110 Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati.. |
|||
Density | 3.11 g/cc | 0.112 lb/in³ | DIN EN 623-2 |
CeramTec Rocar® ST Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Goodfellow Alumina/Silica SiO2 20/Al2O3 80 A continuous multi-filament yarn similar to those made wholly from alumina, relative to which it has a lower upper-use temperature but is more flexible. Similarly, it is used for composites and ther.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | ASTM C20 |
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2) Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Epoxyset Epoxiohm EO-24 Electrically Conductive Epoxy Adhesive EO-24 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management applica.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy .. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance .. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Advanced Ceramics ACL 2088 Zinc Alumino-Silicate A low expansion glass-ceramic suitable for sealing to molybdenum.Information provided by Advanced Ceramics Limited (ACL) |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | ASTM D1475 |
Aptek 2210A/B Electrically conductive urethane adhesive Electrically conductive urethane adhesive, silver-filled, flexible low modulus, low outgassingAPTEK 2210-A/B is a two component, silver-filled, urethane adhesive designed for application where flexi.. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Ceradyne Ceralloy® 147-1E Silicon Nitride Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradynes .. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Mo-Sci Corporation GA-40-I Green A Filter Glass Applications: Lead-free NVIS Green A filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
Density | 3.10 g/cc | 0.112 lb/in³ | |
Mo-Sci Corporation GA-80-N Green Filter Glass Applications: Lead-free NVIS green filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation. |