Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.05 - 3.15 g/cc | 0.110 - 0.114 lb/in³ | ASTM D792 |
Polikim EFALON® B-40 PTFE, 40% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Density | 3.04 g/cc | 0.110 lb/in³ | |
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | Apparent |
Gouda Vuurvast AC 85-5 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. A good volume stability at very high temperatures. Application: chemical incinerators, combustion chambers for very high temperatur.. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | Apparent |
Gouda Vuurvast AK 90 Dense Refractory Brick Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine.. |
|||
Density | 3.05 - 3.12 g/cc | 0.110 - 0.113 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G416 Polytetrafluoroethylene 40% Bronze, 2% Carbon PTFE G Special Compound with bronze Properties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
Schott N-BAF52 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
Schott N-BAK4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
Schott N-SF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
3M Nextel™ 440 Industrial Ceramic Fiber Chemical composition above is wt%. Crystal phases are gamma alumina + mullite + amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural ap.. |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
3M Nextel™ BF-30 Woven Fabric 440 Information provided by 3M |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
3M Nextel™ BF-20 Woven Fabric 440 Information provided by 3M |
|||
Density | 3.05 g/cc | 0.110 lb/in³ | |
3M Nextel™ BF-40 Woven Fabric 440 Information provided by 3M |
|||
Density | 3.04 g/cc | 0.110 lb/in³ | |
Schott N-KZFS5 Glass Information Provided by SCHOTT North America, Inc. |