Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.85 g/cc | 0.103 lb/in³ | Apparent |
Gouda Vuurvast AK 85 P1 Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. In order to optimized the resistance against aluminum attack the sum of Al2O.. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | Apparent |
Gouda Vuurvast LP 80 A Dense Refractory Brick Description: LP 80 is a low porosity brick based on sintered bauxite with an extremely high abrasion resistance and therefore very well suited for application in rotary cement furnaces.Remarks: This.. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | |
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | |
Kaiser 7068 T6, T651 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | |
Kaiser 7068 T6, T6511 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | |
Kaiser 7068 T76, T76511 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | Apparent |
Gouda Vuurvast AK 85 M Dense Refractory Brick Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that.. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | Apparent |
Gouda Vuurvast AK 85 PW Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average.. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Schott N-BAK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Schott N-SF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | |
Schott UG5 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | |
Goodfellow Aluminum-Copper/SiC Metal Matrix Composite Information provided by Goodfellow. |
|||
Density | 2.85 g/cc | 0.103 lb/in³ | |
Alcoa QC-10® Aluminum Mold Alloy Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-.. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Alcoa 7055-T7751 Aluminum Plate Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures.. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Alcoa 7055-T77511 Aluminum Extrusions Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures.. |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
CRP Technology 8601 Aerospace Grade Power Metallurgy Aluminum Alloy For Motorsport and Aerospace marketplaces: manufactured by a special powder metallurgy process using a high-energy mixing process which ensures excellent mechanical properties.Super Aluminium materi.. |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Arlon AR1000 Glass, PTFE and Micro-Dispersed Ceramic Used in the RF and microwave industries.Information provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Aleris Weldural Aluminum Alloy, 400 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Aleris Weldural Aluminum Alloy, 600 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Aleris Weldural Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Aleris Weldural Aluminum Alloy, 200 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Aleris Weldural Aluminum Alloy, 300 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Aleris Weldural Aluminum Alloy, 500 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Density | 2.84 g/cc | 0.103 lb/in³ | |
Aleris Weldural Aluminum Alloy, 700 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Schott BG20 Band Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BC36 |