Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.649 g/cc @Temperature 20.0 °C |
0.09570 lb/in³ @Temperature 68.0 °F |
|
Mateck Quartz Crystalline (SiO2) Optical crystals |