Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.255 g/cc | 0.08147 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® 20FLCA PTFE; Calcium Fluoride Filled
(discontinued **) Data provided by the manufacturer.20 wt.% Calcium Fluoride. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, .. |
|||
Density | 2.255 - 2.265 g/cc | 0.08147 - 0.08183 lb/in³ | |
Mateck Highly Oriented Pyrolytic Graphite Oxidic single crystals. Applications include:Scanning tunneling microscopy-callibration and substratesGraphite monochromatorsx-ray diffractionneutron scattering and diffraction |
|||
Density | 2.255 - 2.265 g/cc | 0.08147 - 0.08183 lb/in³ | |
Momentive Performance Materials HOPG Graphite Monochromator Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-r.. |