Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.20 g/cc | 0.0795 lb/in³ | Green |
Nabaltec NABALOX® NO 613-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
LNP Konduit® OTF-212-11 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D4894 |
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Ferro IX 2693 Dental Glass Glass Type: Fused Silica Typical Application: Low Expansion Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also m.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | estimated by MatWeb |
Garlock GYLON® 3530 PTFE Gasketing, Graphite Filler PTFE with graphite fillerGraphite-filled PTFE offers extremely low void content for minimal emissionsBlack GYLON® delivers long service against volatile hazardous pollutants (VHAP and VOC)Withsta.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Apparent |
Gouda Vuurvast B Sp Dense Refractory Brick Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples .. |
|||
Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon® |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0179 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0179 beads include: calibration, high temperature spacer material for gauge control,.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0186 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0186 beads include: high temperature spacer material for gauge control, coating, fil.. |
|||
Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | |
Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres Appearance: Solid borosilicate glass microspheres with metallic copper coatingTypical applications of GL-0263 glass microspheres include: conductive filler for plastic, pigment, and etc.Information .. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Momentive Performance Materials Type 214 Fused Quartz Tubing Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P1 Acid Vapor Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 832.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P3 Tetrafluoromethane Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 832.6 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Schott LITHOSIL-Q Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
SGL Carbon Group EK 3245 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Chesterton ARC 5ES Rapid Repair Stick Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The AR.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Cured |
Chesterton ARC 890 Course Grade Sliding Wear Compound An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at the thickness of 6 mm (1/4”).. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Cured |
Chesterton ARC BX1 Sliding Wear Compound Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Cured |
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a th.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Brandenburger BL 70 Slide Bearing Material BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%) Excellent thermal shock properties and thermal conductivity when in contact with molten metal. Available as tube, sheath, or rod up to 6 ft (1.9 m) long with diameters 0.6" to 3.75".Information pro.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
LNP Konduit® OTF-212-11 BK8-115 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PH0220AC PA 6 (Europe-Africa-Middle East) LNP* Thermocomp* PH0220AC is a compound based on Nylon 6 resin containing High Specific Gravity Filler. |