Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 6002 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 10-20/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 10-30/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 20-30/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 20-40/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 30-50/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 8-15/3-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: < 8/2-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 10-20/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 8-15/3-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 - 2.30 g/cc | 0.0759 - 0.0831 lb/in³ | |
Pyrotek Bonded Particle Filtration Media Bonded particle filtration media is a proven and efficient means for removing oxides from molten aluminum and its alloys. This filtration media is available in either high strength alumina oxide or.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Rogers Corporation RO3035 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits:Low dielectric lossExcellent mechanical properties versus temperature - reliable stripline and multi-layer board constructions.Uniform mechanical properties- ideal for multi-la.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 30-50/5-15 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Parker Chomerics CHO-FLEX 602 Conductive Coating CHO-FLEX™ 602 is a two-component silver-filled polyurethane coating designed for room temperature or oven cure. CHOFLEX™
602 coating can be sprayed on large panels, cured at room temperature and .. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | typical |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | Apparent |
Gouda Vuurvast B Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1300°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 123 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Goodfellow Leachable Ceramic (Silica, Zircon, Alumina) SiO2 50/ZrSiO4 40/Al2O3 10This form of ceramic is used in the precision foundry industry. The tubes and rods are incorporated into molds in the lost wax process. Using this technique, very fine tole.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insul.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Zircar Refractory Composites RSLE-57 Refractory Sheet ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This material was designed for use as a high strength insulator in induction hot press appl.. |
|||
Density | 2.10 - 2.50 g/cc | 0.0759 - 0.0903 lb/in³ | |
Du-Co Ceramics DC-187 Magnesium Oxide Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.10 - 2.18 g/cc | 0.0759 - 0.0788 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® 52FR Polyester Elastomer TPC-ET
(Unverified Data**) Concentrate in 55 Shore D Polyester Elastomer Carrier Developed for Improving Flame RetardancyInformation provided by DuPont Performance Polymers |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Arlon AD300A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D1505 |
Arlon CuClad 6700 Bonding Film Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu.. |
|||
Density | 2.10 - 2.20 g/cc | 0.0759 - 0.0795 lb/in³ | apparent |
Beijing Evergrow Resources PTFE Extrusion Tube Features:PTFE extruded tubing is manufactured by high pressure PTFE dispense resin mixed with additive, it is extruded and sintered. According to different demands, the tubing could be opaque or tra.. |
|||
Density | 2.10 - 2.30 g/cc | 0.0759 - 0.0831 lb/in³ | |
Beijing Evergrow Resources PTFE Gasket PTFE gasket is manufactured by molding method with PTFE granular resin. PTFE compared with other plastics, has a superior properties against chemicals and temperature. Because of such excellent prop.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | True Density measured via nitrogen gas displacement pycnometer |
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere Fine particle white spheres developed as filler for paints, coatings and films.Information provided by Potters Industries. |