Polymer Property : Density = 0.0755 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.09 g/cc
0.0755 lb/in³
ASTM 1457-62 T
Fluorseals PTFE 25% carbon filled
Improved compressive strength, wear resistance and thermal conductivity.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Density 2.09 g/cc
0.0755 lb/in³
Real Density
SGL Carbon Group CF 1135 Carbon Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Density 2.09 g/cc
0.0755 lb/in³
Saint-Gobain Rulon® 125 Bearing/Seal PTFE
Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.Information provided by distributor TriStar Plastics Cor..
Density 2.09 g/cc
0.0755 lb/in³
ASTM D792
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy
Epiall 1904B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided ..
Density 2.09 g/cc
0.0755 lb/in³
ASTM D792
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced
Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent..
Density 2.09 g/cc
0.0755 lb/in³
ASTM D792
Solvay Specialty Polymers Algoflon® 35CAR PTFE; Petroleum Coke and Graphite  (discontinued **)
Data provided by the manufacturer.35 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p..
Density 2.09 - 2.14 g/cc
0.0755 - 0.0773 lb/in³
extruded; ASTM D792
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite
PTFE G Standard Compound with graphite.Properties: Extremely low coefficient of friction. Fairly good compressive strength. Enhanced chemical resistance. Good wear resistance. Good thermal diss..