Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.952 g/cc | 0.07052 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Density | 1.952 g/cc | 0.07052 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Asia Pacific) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Density | 1.952 g/cc | 0.07052 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Europe-Africa-Middle East) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |