Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.95 g/cc | 0.0704 lb/in³ | |
3M Dyneon™ THV™ 200P Fluorothermoplastic, Powder Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
3M Dyneon™ THV™ 200G Fluorothermoplastic, Pellet Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | EN 60893 |
HOS-Technik Homide 250 Bismaleimide Resin Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Manifattura Cattaneo RULON® J Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
IDI Composites 44-1 Thermoset Polyester, Molding Multi-purpose medium strength material with excellent moldability and low cost.Data provided by the manufacturer. |
|||
Density | 1.95 - 2.22 g/cc | 0.0704 - 0.0802 lb/in³ | Apparent Density |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | typical |
Momentive Performance Materials HBC Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D572 |
Haysite 20000 Polyester BMC, 15% Glass Reinforced The 20000 series bulk molding compound is an electrical grade that can be compression, transfer, or injection molded. Offering good arc/track properties and mechanical strength, this grade is also r.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO R 1183 |
Multibase Multibatch® ME 50062 Anti-blocking Masterbatch LDPE. 80% CaCO3FilledVery Highly FilledInformation provided by Multibase |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific) This material is mineral filled PPO grade with high dielectric constant and low loss tangent |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific) LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound Improved Crack Resistance & Bond Strength. High Temperature Resistance, Thermally Conductive, Low Viscosity. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
Zircar Ceramics AL-CEM Alumina Cement Type AL-CEM Alumina Cement is a high purity alumina bonding agent used for bonding ZIRCAR® fibrous ceramic products to themselves, and as a coating cement to improve the hardness and oxidation resi.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America TEM 9053C Hardware Grade Epoxy Short fiberglass and mineral filled, toughened epoxy molding compound with excellent dimensional stability and high strength properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183A |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi.. |