Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.91 g/cc | 0.0690 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | |
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | |
Cookson Group Plaskon® SMT-B-1FX (146.801) Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It is a reduced catalyst version of SMT-B-1F and provide.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | |
Industrial Laminates/Norplex MC511A Glass Fabric Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | |
LATI Laticonther 62 CPG/500 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | |
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Y H-VAC 40/11 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Y45 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® YPL1500 PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® YR PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America RX® 2-520 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp MH0200A PP (Europe-Africa-Middle East) LNP* Thermocomp* MH0200A is a compound based on Polypropylene resin containing High Specific Gravity Filler.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D792 |
Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ASTM D792 |
Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher t.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ISO 1183 |
Eurostar Starpylen HU 70E3 HDPE, Injection Molding Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ISO 1183 |
Eurostar Starpylen MH0200A HDPE, Injection Molding Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | ISO 1183 |
LATI LARTON CE/60 60% Special Mineral Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America FS-10-VO-200-P Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound with excellent heat resistance.Meets the requirements of ASTM D5948 Type SIG-F.Information provided by Vyncolit.. |
|||
Density | 1.91 g/cc | 0.0690 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 TYPE SIG.Information provided by Vyncolit, a Sumitomo Bak Group |