Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.848 g/cc | 0.06676 lb/in³ | |
Pyrotek TS-550 Insulating Board TS-550 is phenolic-based, fiber and mineral reinforced, high-temperature material. TS-550 offers the high strength and wear resistant properties of laminated materials, while also offering the form.. |