Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.77 g/cc | 0.0639 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N5000 BT Epoxy Laminate and Prepreg The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and .. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**) Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 1700 High Viscosity PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 850 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 2950 PVDF Copolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Conditioned) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Density | 1.77 g/cc @Temperature 25.0 °C |
0.0639 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Techmer ES HiFill® PVDF CF15-M BK 15% Milled Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
UCAR Carbon UCAR® CSX Extruded Graphite Densified prior to graphitization, Grade CSX is an extruded graphite, higher in strength and lower in permeability than CS. It is a material for applications requiring higher densities, better mecha.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | Relative Density; ISO 1183 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D792 |
Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive) Non-sloughing carbon-fiber-filled material with resistance to most chemicals and solvents mechanically strong and tough, thermally stable to 335F, flame and abrasion resistant, and easily fabricated.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® 46HF5040 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ISO 1183 |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65 Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
Cytec Thornel® T-650/35 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ISO 1183 |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
Arkema Group Kynar® 1000 HDC N 118 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1C,P.?E5.I.B.E.C,, ?(1.5-2.5)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, hig.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | |
Arkema Group Kynar® FLEX 2821 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (2.5-6.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousn.. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | Nominal Laminate |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581 Fiber: E-Glass, Weave: 8HS, 300 g/m2Information provided by HexCel |
|||
Density | 1.77 - 1.80 g/cc | 0.0639 - 0.0650 lb/in³ | Average value: 1.79 g/cc Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% .. |
|||
Density | 1.77 g/cc | 0.0639 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat.. |