Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 7518 C Natural Polypropylene Unspecified filler/ reinforcment, 75% by weight.Forms:PelletsInformation provided by Multibase |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated |
|||
Density | 1.74 - 2.06 g/cc | 0.0629 - 0.0744 lb/in³ | Average value: 1.83 g/cc Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO R 1183 |
Multibase Multibatch® ME 50004 Anti-blocking Masterbatch LDPE. 70% CaCO3 FilledInformation provided by Multibase |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 50004 Anti-split HPP. 70% CaCO3 Filled.Thermal Resistance.Information provided by Multibase |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic RX 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Toho Tenax Besfight® G40-600 12K IMA-7C EP03 Continuous Filament Carbon Fiber Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Zeus EFEP Tubing |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Plenco 5350 Phenolic, Granular, Compression Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Cosmic Plastics D45 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Unitika UNILATE® 1 NC PET Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
Eurostar Starflam RF0023K PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023K is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding, Crosslinkable under Beta or Gamma RadiationInformation provided by Euros.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry) Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Applied Composites 175 Vinylester SMC Industry Application: TransportationProduct Application: Structural ExteriorDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
LNP Konduit® OTF-202-10 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically Conductive, Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; h.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |