Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific) LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced Vypet VNT 840 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric Strength Features: High temperature performan.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO R 1183 |
Multibase Multibatch® ME 50008 Anti-blocking Masterbatch LDPE. 70% Silicate Filled. Clarity IRInformation provided by Multibase |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | |
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
Saint-Gobain Meldin® 7003 CM Compression Molded MoS2 Filled Polyimide Melidin® 7003 CM is a compression molded polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions.Specific.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR40 NL100 PBT, 40% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFORM C 3090(K) POM Copolymer, 27% glass fiber reinforced POM-GF27Information provided by BARLOG plastics GmbH. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | cured 14 days @ 50% RH; AMS-S-8802 |
3M AC-240 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | AMS-S83318 |
3M AC-250 A-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | |
BASF Heligoen® Blue L 7072 D Color Additive Description: ß-phthalocyanine blue with excellent dispersibilityChemical Structure: Cu-phthalocyanine, betaPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate s.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | |
BASF Heligoen® Blue L 7081 D Color Additive Description: Easy to disperse ß-phthalocyanine blue with good bronzing stability and extremely reddish flopChemical Structure: Cu-phthalocyanine, betaPhysical form: PowderSuitable for: Baking syste.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D792 |
Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced A copolymer acetal reinforced with 30% glass fiber for use in applications requiring great strength and rigidity.Data provided by the manufacturer, Chem Polymer. |
|||
Density | 1.61 g/cc @Temperature 23.0 °C |
0.0582 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-201-G25 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183-1 |
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data) This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s.. |
|||
Density | 1.61 g/cc | 0.0582 lb/in³ | cured 14 days @ 50% RH; AMS-S-8802 |
3M AC-240 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |