Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.59 g/cc | 0.0574 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued ** The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Plenco 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 5303 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in appliance, automotive and electrical applications. It can be molded by compression, transfer or i.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 50% Filler by WeightAppearance: BlackTPCI# 9809102Information provided by TP Composites, Inc. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP 0159 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF006L PA 66 LNP* THERMOCOMP* RF006L is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF006LXP PA 66 LNP* THERMOCOMP* RF006LXP is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GF1750-N1 50% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Covestro Baydur® STR/C-405 IMR Polyurethane Composite SRIM Foam, 45% Glass Filled, MDI-based 2-Component Liquid System Contains continuous strand fiberglass mat.0.118 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55 Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50 Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 GB6 POM 30% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 500 GB6 POM 30% glass beads filled low viscosity grade with very high stiffness and hardness with lowered shrinkage combined with easy molding of complicated shapesInformation provided by Zakłady Azotowe w .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East) LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Polyplastics Duracon® GH-25D Acetal Co-polymer (POM), GF 25% reinforced, High flow, High strength, High rigidity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Plenco 51030 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
LATI LARAMID G/50 50% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Polyplastics Duracon® GH-25 Acetal Co-polymer (POM), GF 25% reinforced, High strength, High rigidity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |