Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.5 g/cc | 0.054 lb/in³ | ASTM D792 |
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance.. |