Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.439 g/cc | 0.05199 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 3413R PC (Asia Pacific) Lexan* resin 3413R is a flame retardant polycarbonate grade with 30% glass fiber reinforcement to meet UL 94 V1 listing at 1.5mm. This grade can be considered for applications requiring higher stiff.. |
|||
Density | 1.439 g/cc | 0.05199 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 3433R PC 30% GR, provides improved mechanical properties. UV-stabilized. Internal mold release. |