Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.44 g/cc | 0.0519 lb/in³ | Laminate Density |
Hardwire 3x2-4-12 Low Density Composite The 3x2 Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3x2 wire cord is made by twisting 5 individual wire together - three straight filam.. |
|||
Density | 1.44 g/cc | 0.0519 lb/in³ | |
Aremco Pyro-Paint™ 634-AS High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Density | 1.44 g/cc | 0.0519 lb/in³ | |
Abatron AboCast 8708-10 One-Component Structural/Dielectric Epoxy AboCast 8708-10 is a highly filled, class H (180°C) structural, castable adhesive compound for FAST high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Em.. |
|||
Density | 1.44 g/cc | 0.0519 lb/in³ | |
Abatron AboCast 8708-6 One-Component Structural/Dielectric Epoxy AboCast 8708-6 is a highly filled, class H (180°C) structural, castable adhesive compound for SLOW high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Emb.. |
|||
Density | 1.44 g/cc | 0.0519 lb/in³ | |
Abatron AboCast 8708-9 One-Component Structural/Dielectric Epoxy AboCast 8708-9 is a highly filled, class H (180°C) structural, castable adhesive compound for FASTER high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; E.. |
|||
Density | 1.44 g/cc | 0.0519 lb/in³ | |
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200.. |