Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.43 g/cc | 0.0515 lb/in³ | |
Lord Adhesives 306 High Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |