Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 1.39 g/cc | >= 0.0502 lb/in³ | Pycnometer test |
Invista 2201U Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC (Asia Pacific) LNP* LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66 LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6 LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66 LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | |
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound Long aramid fiber reinforced BMI molding compound suited for very demanding tribologic applications under medium to poor lubricated conditions, high temperatures & PV levelsInformation provided by S.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ASTM D792 |
Toyobo T-422T Nylon, Mineral-Reinforced Key Feature: High heat distortion and good toughnessInformation provided by Toyobo Co., Ltd |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring .. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 500T BK602 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T BK602 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications su.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® EB31 Polyester Film, 92 Gauge Mylar® EB31 is a smooth, matte polyester film. It does not contain any plasticizers. General Product Info: Mylar® EB31 has low haze and intermediate gloss. This offers more realistic colors and cl.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® M461 Polyester Film, 48 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® M461 Polyester Film, 75 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® M461 Polyester Film, 92 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® OL2 Polyester Film, 100 Gauge Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® P25 Polyester Film, 75 Gauge Product Description: Mylar® P25 is an uncoated, transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. S.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® RL31 Polyester Film, 100 Gauge Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® RSX Polyester Film, 500 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® RSX Polyester Film, 92 Gauge Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Typical Mylar®; ASTM D1505 |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 105 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ASTM D1505 |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | Pycnometer |
Bapolene® 82 Polyethylene Terephthalate Applications: Water bottles, household, liquor and food containers. All data is based on molded plaques. |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ASTM D792 |
Chem Polymer Chemlon 233 G Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 6 offering excellent high temperature performance, dimensional stability, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 182 Flexible PVC, Sheathing Lead Free Sheathing coaxial cable (90°) |
|||
Density | 1.39 g/cc | 0.0502 lb/in³ | ASTM D792 |
Plenco 3557 Phenolic, Granular, Transfer Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |