Polymer Property : Density = 0.05014 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.388 g/cc
0.05014 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Density 1.388 g/cc
0.05014 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific)
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Density 1.388 g/cc
0.05014 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON EX08318C PEI (Asia Pacific)
LNP* Stat-Kon* EX08318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati..