Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Density | 1.32 - 1.39 g/cc | 0.0477 - 0.0502 lb/in³ | Average value: 1.35 g/cc Grade Count:3 |
Overview of materials for Phenolic, Graphite Cloth Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum value.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | |
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | |
LATI Latilub 87/28-20T PC, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE.Information provided by Lati Industria Termoplastici S.p.A. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183/A |
Solvay TECHNYL® C 52G1 V20 PA6, Conditioned Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 9075 PEI (Europe-Africa-Middle East) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PC SS15 FR BK 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass Fiber, 50% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
Stir SpA TP 78 GE OIL (PVC) Application: Extrusion petrol-tight tubesInformation provided by STIR SpA |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Techmer ES HiFill® HDPE LGF50 12 mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Westlake Plastics Zelux® CN-P Polycarbonate (conductive) Carbon-powder-filled with high flexural strength and good thermal stability to 275F. The CN-P is UL94 V-0 rated at 0.030" and is thermoformable in thinner gauges (0.010"-0.060").Information provide.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | |
Eastman Eastapak 9921 PET ISO data as provided by the manufacturer, Eastman Chemical |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® S610SF BK851 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-96BHT Compression Molded PEEK HT, Unfilled, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight w.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
Eurotec® Tecolen® CP10 GR50 NL PPCP, 50% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | Side 2, Silicone Property; Arlon SQA-TMS-024 |
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight develo.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Stat-kon DE006P PC (Europe-Africa-Middle East) LNP* Stat-kon* DE006P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the .. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
Victrex® Vicote® 701 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |
|||
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
Victrex® Vicote® 707 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |