Physical Properties Metric English Comments
Density 1.268 g/cc
0.04582 lb/in³
Saint-Gobain Chemfab® 250F PTFE Coated Beta Fiberglass Conveyor Belting
Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi..
Density 1.268 g/cc
0.04582 lb/in³
Saint-Gobain Chemfab® 250GW PTFE Coated Beta Fiberglass with Woven-in Graphite Conveyor Belting
Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi..
Density 1.268 g/cc
0.04582 lb/in³
Saint-Gobain Chemfab® 500F PTFE Coated Beta Fiberglass Conveyor Belting
Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi..