Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 104R PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant in limited colors.Effective January 15.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 123R PC (Europe-Africa-Middle East) LEXAN 123R is a low viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 123R is available in transparent, translucent and opaque colours. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL6013 PC (Europe-Africa-Middle East) LEXAN EXL6013 is especially developed for applications requiring a high impact performance combined with an improved chemical resistance over standard polycarbonate. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific) Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® IR1840 PC (Europe-Africa-Middle East) IR1840 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Asia Pacific) Lexan LUX9616G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requirem.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® ML7687 PC (Europe-Africa-Middle East) ML7687 is an optical quality, high purity PC resin optimized for use in optical applications such as light guide panels |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® OQ4320 PC (Europe-Africa-Middle East) LEXAN OQ4320 is a medium viscosity grade with a UV cut-off up to 400 nm and a greater optical purity than standard grades. Fields of application for this material are optical lenses, f.i. in sunglas.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 950 PC (Europe-Africa-Middle East) LEXAN 950 is a high viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 955A PC (Europe-Africa-Middle East) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A is available in transparen.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | |
Meilian Chemical UN3040 BLACK MASTERBATCH BLACK UN3040 contains high opacity carbon black that can provide products with optimum jet blackness and high gloss levels. Its carrier resin is specially designed for use in engineering plastics to.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | |
LATI Latistat 66-06 PA66 Dissipative product based on Polyamide 66 (PA66). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183/B |
Styron CALIBREâ„¢ 302V-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-15 Series Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products a.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM Data |
Styron CALIBRE™ 603 5 Polycarbonate, Branched CALIBRE® 603 is a branched polycarbonate resin and is equipped with a mold release and a UV stabilization package. CALIBRE 603 resins exhibit an excellent property balance of high clarity, high m.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | GB/1033 |
Zhejiang Juner PC-A1 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTACARB 1601 OPALE Polycarbonate Polycarbonate for injection moldingOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
Covestro Desmopan® 385 S Polyurethane injection molding gradehydrolysis-stabilizedhigh mechanical strengthApplicationTechnical partsScreenpacksAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 910-20R##-P0 0.010" (0.254 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 2” Wide Rectangular .2 inch wide, 10 mil thick, Red, Rectangular cross-section, Self-fus.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | B Component; ASTM D1475 |
Aptek 6103-A/B Epoxy Encapsulant Optoelectronic grade, reddish black encapsulant for IR LED discreets. Transparent to IR light while blocking out visible light.Part A is deep red. Part B is clear to pale yellow.Information provided.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade Information provided by Bhansali |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 915-07R##-P1 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.75” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness a.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® FXG154 PC (Europe-Africa-Middle East) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |