Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.174 g/cc | 0.04241 lb/in³ | Melt Density |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |