Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 F Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, highly crystallized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
Nilit RECONYL B Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
Polykemi AB SCANMID 6 B12^ FC Nylon 6 Information provided by Polykemi AB |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ±0.02 g/cm³; DIN 53479 |
PolyOne Bergamid™ A700 BK VN4255 LS Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ±0.03 g/cm³; DIN 53479 |
PolyOne Bergamid™ B70 red RAL3001 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
PolyOne Edgetek® MP-10GF/000 Modified PPO - 10% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
LATI LATISTAT 30/R-05 High Impact Strength Polystyrene Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO data |
BASF Capron® 1202CQ Nylon 6 (Dry)
(discontinued **) Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | (Dry) |
BASF Capron® 8203C Nylon 6 (Conditioned)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 E U Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: ExtrusionTPCI# 9777102Information provided by TP Composites, Inc. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Chase Plastics CP Pryme® N100HL (Dry) Nylon 6, Heat Stabilized, Lubricated Features: Heat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
Wellman Wellamid® 42LH-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Density | 1.13 - 1.20 g/cc | 0.0408 - 0.0434 lb/in³ | FTTC 2443 |
Formosa Plastics 10% Sodium Hypochlorite Information provided by Formosa Plastics Corporation, USA |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTAPROP H 2550 CBS/E Polypropylene, 25% Mineral Filled PP homopolymer 25% mineral fillerHigh gloss, very high melt flow rate, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | dry; ISO 1183 |
DSM Akulon® F232 PA6 Medium/High Viscosity, Extrusion Grade |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | dry; ISO 1183 |
DSM Akulon® K125/A PA6 Low Viscosity |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
DSM Fibre Intermediates Nyrim® 4000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Density | 1.13 - 1.17 g/cc | 0.0408 - 0.0423 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 39/T Flexible PVC, Injection Molding for Footwear Sandals |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ASTM D792 |
3M Scotchcast™ 3570G-N Connector Sealing Pack The 3M Scotchcast Connector Sealing Pack 3570G-N insulates and provides protection for electrical spring connectors against dust, soil, water, and other environmental elements. Each sealing pack con.. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® F136-E Nylon 6 (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
BASF Nypel® 2314 HS BK6 PA6 (Dry) Description: Nypel® 2314 HS BK6 is a black pigmented, low viscosity, heat stabilized, semi crystalline, injection molding compound based on recycled PA6 feedstocks. It also offers the following: go.. |