Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
Nylene® PX1719 Nylon 6 Dry as molded. Extrusion grade. Nylene PX1719HS is a heat stabilized, high impact, nylon 6 extrusion grade resin with a low flexural modulus. PX1719HS is ideally suited for extrusion of tubing and.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Polykemi AB POLYblend 6005B UV PC/ABS-Blend Information provided by Polykemi AB |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Polykemi AB POLYelast TPE Z805P Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Polykemi AB SCANAMID 66 A52^E Nylon 66, Modified Information provided by Polykemi AB |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
PTS Trimid® N66-T100 Toughened Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | STN EN ISO 1183-1 |
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Density | 1.08 - 1.45 g/cc | 0.0390 - 0.0524 lb/in³ | Average value: 1.18 g/cc Grade Count:43 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
Stellarchem MP-850 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® ABS/PBT 1000 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Styrolution Absolan® 2150 SAN Absolac 2150 Crystal is a heat and chemical resistant gradeInformation provided by Styrolution |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Styrolution Absolan® 2300 Sparkle SAN Absolac 2300 Sparkle is a good flow gradeInformation provided by Styrolution |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
Covestro Desmopan® W DP89043D Polyurethane PreprocessingMax. Water content |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
BASF Ultramid® 8255 HS PA6 (Dry) Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and
fle.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 261WO PPO A general purpose V-0 rated resin with good impact strength.Data provided by the manufacturer |
|||
Density | 1.08 - 1.12 g/cc | 0.0390 - 0.0405 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 465A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
A. Schulman ComAlloy Comtuf® 101 Polypropylene, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.25% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Density | >= 1.08 g/cc | >= 0.0390 lb/in³ | |
3M Scotch-Weld™ TS115 HGS Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
Von Roll Isola IMI Varnish 707 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 46°C. Usag.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
BASF Luranyl® KR 2451/3 Polyphenylene Ether + Styrene-Butadiene Blend Especially easy flowing grade containing halogen-free, flame-retardant; mainly used for housings for electrical equipment and in the electronics sector.Data was collected by ISO methods and provided.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | |
Solvay RHODAPEX® ESC-70/AB Surfactant Chemical Name: Sodium Laureth SulfateCAS: 68585-34-2Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX ESC-70/AB is used in the formulation of high quality sh.. |
|||
Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |