Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron AP-78 EP ABS Electro Plating Applications Electroplating & Hot Stamping GradesInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications Electroplating & Hot Stamping GradesInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron TG-3(M) ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron HI-34 ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron HR-60 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade Very High Flow, Medium Impact GradeInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron HI-34 ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron HCR-15 M ABS Heat Resistant Chemical Resistant GradeInformation provided by Bhansali |
|||
Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade Medium Impact, High Gloss, High FlowInformation provided by Bhansali |